bobburito Posted August 1, 2014 Share Posted August 1, 2014 i found what looks to be a possible hairline crack im not sure i would really love some feedback thanks Link to comment Share on other sites More sharing options...
bobburito Posted August 1, 2014 Author Share Posted August 1, 2014 Link to comment Share on other sites More sharing options...
BirdMobile Posted August 1, 2014 Share Posted August 1, 2014 That looks like a casting mark to me... Link to comment Share on other sites More sharing options...
JuhaKankkunen Posted August 1, 2014 Share Posted August 1, 2014 it doesn´t seems to be a crack for me. Its only a defect on the aluminium. Link to comment Share on other sites More sharing options...
BlackBoot Posted August 1, 2014 Share Posted August 1, 2014 That's a casting mark, I have a crack in my block on my wagon it's easy to see it gathers dirt in the crack. I had JB Weld holding it closed for 2 years! Link to comment Share on other sites More sharing options...
Prwa101 Posted August 1, 2014 Share Posted August 1, 2014 It's an imperfection from the cast and mold. 100% sure. Nothin to worry about Prwa Link to comment Share on other sites More sharing options...
bobburito Posted August 1, 2014 Author Share Posted August 1, 2014 Mind you this is my first subaru teardown lol so bare with me just want to make sure I do it right Link to comment Share on other sites More sharing options...
bobburito Posted August 1, 2014 Author Share Posted August 1, 2014 (edited) Looks like it's time to put her back together! !!! Edited August 1, 2014 by bobburito Link to comment Share on other sites More sharing options...